GECH30 – Coarsely grogged stoneware clay with yellow-beige firing color

The GECH30 is a robust stoneware clay with coarse grog, perfect for handbuilding, slab techniques, object ceramics, and architectural ceramics. The grog ensures high stability, allowing even large and complex shapes to be reliably created. Despite the coarse texture, the clay remains highly malleable and pleasant to work with.

After the stoneware firing, the GECH30 takes on a warm, yellow-beige color, giving it a natural, earthy appearance. The high iron oxide content creates vibrant glazing effects, making the clay especially suitable for artistic surface designs.

In reduction firings, the color further develops a fascinating reddish yellow-brown shade, while glazes interact intensely with the clay. The GECH30 is also highly suitable for the Raku technique: the unglazed surface takes on a rough and matte texture, which is perfect for experimental surface effects.

Benefits of the GECH30:

  • Coarse grog (30% 0-3 mm) ensures high stability
  • Perfect for handbuilding, slab techniques, object ceramics, and architectural ceramics.
  • Warm yellow-beige firing color in stoneware firing
  • Exciting glazing effects due to high iron oxide content
  • Striking reddish yellow-brown shade
  • Ideal for Raku and firing experiments in direct flames

The GECH30 lets you create impressive works with warm colors, vibrant glazing effects, and robust durability – a stoneware clay for creative freedom and exciting experiments.

Addition
ca. 40% Schamotte 0 - 1.25mm
Category
Steinzeug
Drying Shrinkage
ca. 6%
Fir. Col. after Rawburn
lila
Fir. Col. red. after Glossbur
rötlich-gelbbraun
Firing Shrinkage
ca. 4.5% bei 1280°C
Firing colour (oxidation)
gelbbeige
Glossburn
1150 - 1340°C
Grogged
yes
Rawburn
1020°C
Suitable for raku
ja
Water Absorption
ca. 6% bei 1280°C